Product Code:Diameter:Length:Material:
CD F-AHSpecify DSpecify LSpecify
Flanged Acoustical Hanger CD Weld Stud
Flanged Acoustical Hanger (lagging stud) CD Weld Stud
STUD
DLFDHDHLWT
.1681-1/8.250.1877/85/161/16
MATERIALMILD STEELSTAINLESS STEEL
C - 0.23% max.P - 0.04% max.AISI grade - 304/305 std.
Mn - 0.90% max.S - 0.05% max.Other grades available upon request.
MECHANICAL PROPERTIESTensile - 60,000 psi (min.)Tensile - 85,000 psi (min.)
Yield - 50,000 psi (min.)
Yield - 40,000 psi (min.)